Selection, Application, and Disposal of Finishing Fluids Available to Purchase
-
Published:1994
Abstract
Grinding is an extremely complex process that requires the consideration of a number of elements in order to make a reasonably adroit initial selection of a fluid or fluids for a manufacturing plant. In addition, the disposal of grinding wastes must meet the minimum requirements as recommended by the federal Environmental Protection Agency (EPA) and Resource Conservation and Recovery Act (RCRA) regulations. This article explains the selection considerations of such fluids, as well as the applications and environmental issues related to the grinding processes.
Cynthia K. Cordell, Selection, Application, and Disposal of Finishing Fluids, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 158–160, https://doi.org/10.31399/asm.hb.v05.a0001240
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.