Testing of Stability and Thermal Properties of Thermal Barrier Coatings
-
Published:1994
Abstract
This article discusses the various tests applied to a thermal barrier coating system and to the zirconia layer to establish thermomechanical, environmental stability, and thermal design properties such as coefficient of thermal expansion, specific heat, and thermal transport properties. Thermal fatigue testing and the test for evaluating oxidation resistance of the bond coat is also discussed.
Thomas A. Taylor, Ray E. Taylor, Testing of Stability and Thermal Properties of Thermal Barrier Coatings, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 654–659, https://doi.org/10.31399/asm.hb.v05.a0001299