Rust-Preventive Compounds Available to Purchase
Revising author
-
Published:1994
Abstract
Rust-preventive compounds are removable coatings used for the protection of the surfaces of iron, steel, coated or galvanized products, and other alloys. This article describes the basic parts of rust-preventive compounds, namely, carrier, film former, polar materials, and specialty additives. It explains types of rust-preventive compounds, including dry films and water-based dry films. The article also discusses the methods of application of various compounds, such as petrolatum compounds and emulsion compounds. It contains tables that provide information on the characteristics, applications, and physical properties of rust-preventive materials covered by military specifications. Finally, the article describes the various considerations and parameters for selecting rust-preventive materials.
Harry D. Ferrier, Jr., Rust-Preventive Compounds, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 412–420, https://doi.org/10.31399/asm.hb.v05.a0001276
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.