Tin Plating
By
Arthur J. Killmeyer
Arthur J. Killmeyer
Tin Information Center of North America
Revising author
Search for other works by this author on:
-
Published:1994
Abstract
A tin deposit provides sacrificial protection to copper, nickel, and many other nonferrous metals and alloys. Tin also provides good protection to steel. Tin can be deposited from either alkaline or acid electrolytes. This article explains the compositions and operating conditions of these electrolytes.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Arthur J. Killmeyer, Tin Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 239–241, https://doi.org/10.31399/asm.hb.v05.a0001250
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Glossary of Terms: Surface Engineering
Surface Engineering
Weldability of Ferrous and Nonferrous Alloys
Welding Fundamentals and Processes
Plating Adherence Problems in Electronic Components
ASM Failure Analysis Case Histories: Processing Errors and Defects
Bainitic Structures
Metallography and Microstructures
Nonferrous Metals
Elementary Materials Science
Massive Transformation Structures
Metallography and Microstructures
Periodic Table of Elements
Fundamentals of Modeling for Metals Processing
Retrogression and Reaging
Heat Treating of Nonferrous Alloys
Forming of Nonferrous Metals
Metals Handbook Desk Edition (2nd Edition)
Introduction to Structures in Metals
Metallography and Microstructures