Abstract
This article is a compilation of terms related to surface engineering of irons, steels, and nonferrous metals.
You do not currently have access to this chapter.
Citation
Glossary of Terms: Surface Engineering, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 944–973, https://doi.org/10.31399/asm.hb.v05.a0005585
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Macroetchants Based on Copper-Containing Compounds–For Etching of Iron And Steel
Metallography Principles and Practice
Introduction to Steels and Cast Irons
Metallographer’s Guide Practices and Procedures for Irons and Steels
Glossary
Metallographer’s Guide Practices and Procedures for Irons and Steels
Weldability of Ferrous and Nonferrous Alloys
Welding Fundamentals and Processes
Tin Plating
Surface Engineering
Microstructures of Nitrided Iron and Steel
Practical Nitriding and Ferritic Nitrocarburizing
Fundamentals of the Heat Treating of Steel
Practical Heat Treating (Second Edition)
Tables Helpful to the Metallographer
Metallographer’s Guide Practices and Procedures for Irons and Steels
Tables of Chemicals and Etchants
Metallography and Microstructures
Free Energy of Pure Substances
Thermodynamics of Microstructures