Abstract
Commercial zinc plating is accomplished by a number of distinctively different systems: cyanide baths, alkaline noncyanide baths, and acid chloride baths. This article focuses on the composition, advantages, disadvantages, operating parameters, and applications of each of the baths. It provides information on the control of thicknesses of zinc specified for service in various indoor and outdoor atmospheres and on the similarities between cadmium and zinc plating.
You do not currently have access to this chapter.
Citation
A. Sato, Zinc Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 227–235, https://doi.org/10.31399/asm.hb.v05.a0001248
Download citation file:
Related Book Content
Electrodeposition Processes
Metals Handbook Desk Edition (2nd Edition)
Cadmium Plating
Surface Engineering
Fracture of Tempered Leaf Springs
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
High-Strength Structural and High-Strength Low-Alloy Steels
Metals Handbook Desk Edition (2nd Edition)
Failure of Elevator Hinge Pins in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Brittle Fracture of a Cadmium-Plated 4140 Steel Retaining Ring at a Hard Spot Caused by an Arc Strike
ASM Failure Analysis Case Histories: Mechanical and Machine Components
Fatigue Fracture of a Music-Wire Spring Caused by Poor Electroplating Practice
ASM Failure Analysis Case Histories: Processing Errors and Defects
Hydrogen Embrittlement Failure of Socket Head Cap Screws
Handbook of Case Histories in Failure Analysis
Fracture of an Accumulator Ring Due to Hydrogen Embrittlement
ASM Failure Analysis Case Histories: Processing Errors and Defects
Hydrogen Embrittlement of Aircraft Components
ASM Failure Analysis Case Histories: Air and Spacecraft