Compliant Wipe Solvent Cleaners[1]
-
Published:1994
Abstract
Wipe solvents are used to remove contaminants from a workpiece before it undergoes manufacturing operations that require clean surfaces, such as bonding, sealing, painting, welding, plating, specialized surface treatment procedures, and others. This article describes the evaluation parameters for wipe solvent cleaners, including methyl ethyl ketone, methyl isobutyl ketone, trichloroethene, tetrachloroethylene, acetone, toluene, dichloromethane, benzene, xylene, and other alternate wipe solvent cleaners. It contains a table that lists the compositions and properties of wipe solvent cleaners.
Mark T. Carroll, Compliant Wipe Solvent Cleaners, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 940–943, https://doi.org/10.31399/asm.hb.v05.a0001326
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.