Compliant Organic Coatings
-
Published:1994
Abstract
This article discusses coating products available for use in the aerospace industry that are compliant with regulations requiring reductions in emissions from organic solvents. The coating products addressed include primers, topcoats, and chemical milling maskants. It describes their characteristics and limitations compared to conventional noncompliant materials. The article addresses the methods and products commonly used achieve regulatory compliance: waterborne coatings, exempt-solvent-based coatings, high-solids coatings, powder coating, and electro-deposition.
Thomas E. Kearney, Compliant Organic Coatings, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 935–939, https://doi.org/10.31399/asm.hb.v05.a0001325