Vapor Degreasing Alternatives Available to Purchase
-
Published:1994
Abstract
The chemicals that have been used in traditional vapor degreasing have serious health and environmental hazards that have prompted the search for modified and alternative techniques. This article provides a detailed discussion on the regulatory mandates that affect the use of industrial degreasing methods. It describes the aqueous degreasing technique, which forms an attractive alternative to the traditional vapor degreasing process. The article includes information on the materials and equipment used in the process, and discusses the advantages and disadvantages of hot and dip tank systems of aqueous degreasing. It explains how to convert an existing vapor degreaser to an aqueous cleaning system.
Dennis Zupan, Tony L. Green, Donald W. Benjamin, Bruce Hooke, Calvin Fong, Vapor Degreasing Alternatives, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 930–934, https://doi.org/10.31399/asm.hb.v05.a0001324
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.