Abstract
Environmental and worker health regulations have increased the costs associated with cadmium coating application and cadmium-beating waste disposal, thus creating economic incentives for industrial users to seek cadmium plating replacements. This article presents a cadmium replacement identification matrix that includes information on the specifications, corrosion control performance, environment-assisted cracking, coating lubricity, environmental and worker health regulations, and cost and performance factors for various replacement processes.
Mark W. Ingle, Cadmium Elimination in Surface Engineering, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 918–924, https://doi.org/10.31399/asm.hb.v05.a0001322
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.