Elastomeric Coatings for Automotive Plastics Available to Purchase
-
Published:1994
Abstract
This article describes elastomeric coatings that are suitable for painting flexible plastic substrates. It focuses on coatings systems that find utility in automotive exterior applications, where the requirements of appearance and durability are most severe. The article discusses acrylic polyols, condensation polymers, vapor curing systems, water-based coatings, and coatings for thermoplastic olefins.
Robert M. Piccirilli, John Burgman, Elastomeric Coatings for Automotive Plastics, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 448–453, https://doi.org/10.31399/asm.hb.v05.a0001278