Iron has been electroplated from a variety of electrolytes, whose bath parameters result in coatings that have widely divergent characteristics according to the specific characteristics desired in the finished product. This article provides an overview of the process description and processing equipment and discusses the properties, advantages, limitations, and principal applications of iron plating. It also describes the environmental, health, and safety considerations of iron plating.
Sue Troup-Packman, Iron Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 213–214, https://doi.org/10.31399/asm.hb.v05.a0001246