Environmental Regulation of Surface Engineering
-
Published:1994
Abstract
This article describes selected U.S. environmental statutes and regulations that are pertinent to material surface finishers. It provides information on the applicability, requirements, and permitting conditions of the Clean Air Act, the Resources Conservation and Recovery Act, the Superfund Amendments and Reauthorization Act, and the Clean Water Act.
David J. Smukowski, Environmental Regulation of Surface Engineering, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 911–917, https://doi.org/10.31399/asm.hb.v05.a0001321