Surface Engineering
Babbitting
-
Published:1994
Abstract
Babbitting is a process by which relatively soft metals are bonded chemically or mechanically to a stronger shell or stiffener which supports the weight and torsion of a rotating, oscillating, or sliding shaft. This article focuses on workpiece preparation and babbitting methods. Prior to casting, the workpiece must be scrupulously prepared by various cleaning, fluxing, and tinning steps. Babbitting of bearing shells can be accomplished by three methods, namely, static babbitting, centrifugal casting, and metal spray babbitting.