Decorative Chromium Plating
Revising author
Revising author
-
Published:1994
Abstract
Most decorative chromium coatings have been applied using hexavalent and trivalent plating processes that are based on chromic anhydride. This article provides a discussion on chromium electrodeposits and their use as microdiscontinuous coating for corrosion protection. It focuses on the operating conditions of various chromium plating parameters: bath composition, temperature, voltage, anode materials, and current density. These parameters need to be considered for obtaining high quality decorative chromium coatings. An overview of plating problems encountered in chromium plating and their corrections is also provided.
Sign in
ASM members
Member Sign InJames H. Lindsay, Donald L. Snyder, Decorative Chromium Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 192–200, https://doi.org/10.31399/asm.hb.v05.a0001244
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.