Emulsion Cleaning
Revising author
-
Published:1994
Abstract
Emulsion cleaning is an industrial cleaning process that uses an organic solvent as the main active agent. This article provides information on the applications, concerns and limitations, and process parameters of emulsion cleaning. It describes the processing variables and equipment for three main stages of emulsion cleaning: immersion cleaning, secondary cleaning, and spray cleaning. In addition, the classifications, composition, and selection criteria are also discussed.
Steven M. Nourie, Emulsion Cleaning, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 33–38, https://doi.org/10.31399/asm.hb.v05.a0001224