Abstract
Multiple-layer alloy electrodeposition involves the formation of an inhomogeneous alloy consisting of lamellae of different composition. This article reviews the process description, engineering parameters, characterization, and applications of multiple-layer alloys. Pulsed-current plating and pulsed-potential plating are also discussed.
Daniel T. Schwartz, Multiple-Layer Alloy Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 274–276, https://doi.org/10.31399/asm.hb.v05.a0001260