Nickel Alloy Plating
-
Published:1994
Abstract
Nickel alloys electroplated for engineering applications include nickel-iron, nickel-cobalt, nickel-manganese, and zinc-nickel. This article provides the process description and discusses the processing variables, properties, advantages, and disadvantages of nickel-iron, nickel-cobalt, nickel-manganese alloys, and nickel chromium binary and ternary alloys. It also includes information on the environmental, health, and safety considerations for these nickel-base alloys.
S. Alec Watson, Nickel Alloy Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 266–269, https://doi.org/10.31399/asm.hb.v05.a0001258