Glazes and Enamel Coatings for Ceramics and Glasses Available to Purchase
-
Published:1994
Abstract
This article focuses on the ceramic coatings for ceramic and glass substrates. It describes the role of oxides in glazes and discusses the optical and appearance properties of various types of glazes, such as leadless glazes, lead-containing glazes, opaque glazes, and satin and matte glazes. The article provides information on the classification of pigments and the applications of ceramic coatings for decorations on ceramic and glass surfaces.
Glazes and Enamel Coatings for Ceramics and Glasses, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 877–882, https://doi.org/10.31399/asm.hb.v05.a0001316