Continuous Electrodeposited Coatings for Steel Strip Available to Purchase
-
Published:1994
Abstract
This article explains the applications of continuous electroplated steel. For each category of application, the type of coating needed and the key attributes of the coating are discussed. The bulk of the article describes electrodeposition technology, including plating line components and process classification.
Stavros G. Fountoulakis, Continuous Electrodeposited Coatings for Steel Strip, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 349–359, https://doi.org/10.31399/asm.hb.v05.a0001271