Alkaline Cleaning Available to Purchase
Revising author
-
Published:1994
Abstract
Alkaline cleaning is a commonly used method for removing a wide variety of soils from the surface of metals. This article focuses on the composition, operating conditions, and test and control of alkaline cleaners, as well as equipment used and their application methods. It describes the mechanisms of alkaline cleaning, such as saponification, displacement, emulsification and dispersion, and metal oxide dissolution. The article concludes with information of the safety and environmental considerations in the usage of alkaline cleaners.
Gerald J. Cormier, Alkaline Cleaning, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 18–20, https://doi.org/10.31399/asm.hb.v05.a0001222