Zirconium and hafnium surfaces require cleaning and finishing for reasons such as preparation for joining, heat treatment, plating, forming, and producing final surface finishes. This article provides information on various surface treatment processes, surface soil removal, blast cleaning, chemical descaling, pickling or etching, anodizing, autoclaving, polishing, buffing, vapor phase nitriding, and electroplating. Applications of these surface treatment processes are also reviewed.