Book Chapter
Silver Plating Available to Purchase
By
Alan Blair
Alan Blair
AT&T Bell Laboratories
Search for other works by this author on:
-
Published:1994
Page range:
245 - 246
Abstract
Electroplated silver is used in both decorative and functional applications, such as engineering and electrical/electronic applications. This article explains the solution formulations and specifications of electrolytes used in silver plating.
Topics
Silver plating
You do not currently have access to this chapter.
Citation
Alan Blair, Silver Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 245–246, https://doi.org/10.31399/asm.hb.v05.a0001252
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Electroless and Electrolytic Plating Procedures
Metallography Principles and Practice
Gold Plating
Surface Engineering
Iron Plating
Surface Engineering
Electrochemical Machining
Machining
Stray Currents in Underground Corrosion
Corrosion: Environments and Industries
Copper Alloy Plating
Surface Engineering
Lead Plating
Surface Engineering
Electrochemical Grinding
Machining
Electrodeposition Processes
Metals Handbook Desk Edition (2nd Edition)
Design and Fabrication of Inductors for Induction Heat Treating
Induction Heating and Heat Treatment