242 - 244
Abstract
Lead has been deposited from a variety of electrolytes, including fluoborates, fluosilicates, sulfamates, and methane sulfonic acid baths. This article provides a discussion on these electrolytic baths and includes information on the process sequence, equipment requirements, and applications of lead plating.
You do not currently have access to this chapter.
Citation
George B. Rynne, Lead Plating, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 242–244, https://doi.org/10.31399/asm.hb.v05.a0001251
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Chemical Milling
Machining
Gold Plating
Surface Engineering
Iron Plating
Surface Engineering
Electrochemical Machining
Machining
Stray Currents in Underground Corrosion
Corrosion: Environments and Industries
Precoating Operations
Thermal Spray Technology
Indium Plating
Surface Engineering
Electrodeposition Processes
Metals Handbook Desk Edition (2nd Edition)
Silver Plating
Surface Engineering
Photochemical Machining
Machining