Quenching is one of the most important heat treating processes, because it is so closely related to dimensional control requirements and control of residual stresses. This article provides an overview of the fundamental material- and process-related parameters of quenching on residual stress, distortion control, and cracking. This overview is followed by various selected case histories of failures attributed to the quenching process.