Other Quenchants and Quenching Processes Available to Purchase
-
Published:2024
Abstract
This article presents a detailed discussion on the characteristics, types, properties, quenchants, applications, advantages, and disadvantages of various types of quenching: air quenching, water quenching, rinse quenching, time quenching, press quenching, delayed quenching, fluidized-bed quenching, ultrasonic quenching, intercritical quenching, subcritical quenching, ausbay quenching, hot isotactic press quenching, slack quenching, differential quenching, and double quenching.
Xinmin Luo, George E. Totten, Lauralice C.F. Canale, Rosa L. Simencio Otero, Other Quenchants and Quenching Processes, Quenchants and Quenching Technology, Vol 4F, ASM Handbook, Edited By George E. Totten, Rosa Simencio Otero, Xinmin Luo, Lauralice C.F. Canale, ASM International, 2024, p 453–500, https://doi.org/10.31399/asm.hb.v4F.a0007014
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.