Abstract
This article presents the modes of heat transfer and the stages of cooling during quenching. It provides an overview on the wetting process and then focuses on the evaluation of heat transfer during quenching. It also presents the challenges of thermal process evaluation based on an inverse heat conduction analysis. The article contains a compilation of best practice examples on heat transfer evaluation, which are intended to represent the practical aspects and applicability of the methods aiming the prediction of heat-transfer coefficients.
Imre Felde, Heat Transfer during Quenching Processes, Quenchants and Quenching Technology, Vol 4F, ASM Handbook, Edited By George E. Totten, Rosa Simencio Otero, Xinmin Luo, Lauralice C.F. Canale, ASM International, 2024, p 55–68, https://doi.org/10.31399/asm.hb.v4F.a0006997
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.