Abstract
Steels are among the most versatile materials in modifying their microstructure and properties by heat treatment. This article outlines the basic concepts of physical metallurgy relating to the heat treatment of steel. It considers the phases and microstructures of steel together with the transformations observed and critical temperatures during heat treatment. Additionally, the different types of steels, heat treatments, and their purposes are also discussed.
Diego E. Lozano, Gabriela M. Martínez-Cázares, Yaneth Bedolla-Gil, Metallurgical Fundamentals of Quenching, Quenchants and Quenching Technology, Vol 4F, ASM Handbook, Edited By George E. Totten, Rosa Simencio Otero, Xinmin Luo, Lauralice C.F. Canale, ASM International, 2024, p 3–25, https://doi.org/10.31399/asm.hb.v4F.a0006995
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.