Advanced Industrial Quench System Design—Fluid Dynamics Analysis
-
Published:2024
Abstract
Computational fluid dynamics (CFD) provides an efficient, alternate, virtual approach for simulating and analyzing quenching processes with an impact on component design, manufacturing process, and quality. This article provides domain insights for quenching researchers and CFD practitioners for the modeling of the industrial quenching process and for supporting the diverse multifunctional needs in an industry, ranging from primary metallurgical companies (steel, aluminum, and other alloys), original equipment manufacturers, engineering companies, captive and commercial heat treating facilities, quench system manufacturers, and quench fluid suppliers. It describes the governing differential equations for the fluid flow and heat-transfer phenomena during quenching. The article also discusses different modeling categories to determine a CFD methodology for quenching.
Francisco Andrés Acosta-González, Advanced Industrial Quench System Design—Fluid Dynamics Analysis, Quenchants and Quenching Technology, Vol 4F, ASM Handbook, Edited By George E. Totten, Rosa Simencio Otero, Xinmin Luo, Lauralice C.F. Canale, ASM International, 2024, p 356–370, https://doi.org/10.31399/asm.hb.v4F.a0007008
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.