The role of a mixer/agitator in quenching applications is to control the mixing environment in order to meet the process criteria. This article provides the basic fundamentals of the sizing of agitators, tank geometry importance, and other considerations for the application of agitators in quench tanks. It also discusses the differing methods for the sizing and selection of agitators for quench tank applications.