Solder cracking is one of the dominant failure modes of the electronic assembly system. Experience shows that solder joints can fail due to processing defects during solder joint formation or due to excessive loading in various applications. This article introduces major fractography techniques to demonstrate typical solder joint failure and background failure mechanisms. These techniques may be helpful to readers in recognizing failure modes and in preventing further failures during product development and process implementation.