Fractography of Titanium Alloys
-
Published:2024
Abstract
This article presents a detailed discussion on the microstructures, physical metallurgy, classification, deformation behavior, and fracture modes of titanium alloys. It illustrates the effect of microstructure and texture on the fracture topography and fracture behavior of titanium alloys with a variety of relevant examples.
Adam Pilchak, Jim Williams, Fractography of Titanium Alloys, Fractography, Vol 12, ASM Handbook, Edited By Craig J. Schroeder, Ronald J. Parrington, Joseph O. Maciejewski, James F. Lane, ASM International, 2024, p 408–429, https://doi.org/10.31399/asm.hb.v12.a0007034