Abstract
Fracture of aluminum alloys can occur due to several failure types and/or fracture morphologies, including overload, intergranular fracture, fatigue, corrosion, and mixed-mode fracture. This article provides a detailed discussion on these failure types and/or fracture morphologies. It also presents the differences between wrought and cast aluminum products.
Ellen Wright, Fractography of Aluminum Alloys, Fractography, Vol 12, ASM Handbook, Edited By Craig J. Schroeder, Ronald J. Parrington, Joseph O. Maciejewski, James F. Lane, ASM International, 2024, p 352–368, https://doi.org/10.31399/asm.hb.v12.a0007025