Fracture and Fractography of Tool Steels and Bearing Steels
-
Published:2024
Abstract
This article describes some of the underlying factors of tool steel and bearing steel fractures and appearances. It also briefly introduces the general types of cold work and hot work tool steels and their typical performance requirements. This includes the importance of microstructural conditions achieved with powder metallurgy (PM) tool steels and the need for steel “cleanliness,” especially in preventing contact fatigue in bearings or bending fatigue in gears.
Arthur Reardon, Fracture and Fractography of Tool Steels and Bearing Steels, Fractography, Vol 12, ASM Handbook, Edited By Craig J. Schroeder, Ronald J. Parrington, Joseph O. Maciejewski, James F. Lane, ASM International, 2024, p 342–344, https://doi.org/10.31399/asm.hb.v12.a0007029