In this article, a basic summary of fracture mechanisms in carbon and alloy steels is presented, along with numerous examples of these fractures. These examples include ductile fracture, brittle cleavage fracture, intergranular fracture, fatigue fracture, and environmentally assisted failure mechanisms.