Fractography of Cast Irons Available to Purchase
-
Published:2024
Abstract
The cast iron family includes several different groups, including gray iron, ductile iron, compacted graphite iron, malleable iron, white iron, and many different grades within each of these alloy groups. This article addresses issues specific to gray iron, but in many instances the discussion can be related to the other cast iron groups and the various grades within those groups. It discusses the usage of techniques and procedures in cast iron fractography. The article presents a list of common defects that can initiate failure.
Richard B. Gundlach, John M. Tartaglia, Fractography of Cast Irons, Fractography, Vol 12, ASM Handbook, Edited By Craig J. Schroeder, Ronald J. Parrington, Joseph O. Maciejewski, James F. Lane, ASM International, 2024, p 317–325, https://doi.org/10.31399/asm.hb.v12.a0007035
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.