Photography of Fractured Parts and Fracture Surfaces Available to Purchase
-
Published:2024
Abstract
This article provides a discussion on the following photographic equipment: point-and-shoot cameras, digital single-reflex cameras, stand-mounted digital zoom cameras, and digital microscope cameras. It presents two principal types of optical microscopes that are appropriate for visual examination of fractured parts: the stereomicroscope and the single-light-path digital microscope. The common features present on fracture surfaces are each considered separately, both in their significance and as photographic challenges. The article also presents a short note on low-magnification scanning electron microscopy and postcapture image processing.
David M. Christie, Photography of Fractured Parts and Fracture Surfaces, Fractography, Vol 12, ASM Handbook, Edited By Craig J. Schroeder, Ronald J. Parrington, Joseph O. Maciejewski, James F. Lane, ASM International, 2024, p 188–201, https://doi.org/10.31399/asm.hb.v12.a0006846
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.