This article describes the general factors that can influence fracture appearances. The focus is on the general practical relationships of fracture appearances, with factors presented in some broad categories, including: material conditions (e.g., crystal structure and microstructure); loading conditions (stress state, strain rate, and fatigue); manufacturing conditions (casting, metal-working, machining, heat treatment, etc.); and service and environmental factors (hydrogen embrittlement, stress corrosion, temperature, and corrosion fatigue).
George Wildridge, Mark Hineman, Factors Influencing Fractures and Fracture Appearance, Fractography, Vol 12, ASM Handbook, Edited By Craig J. Schroeder, Ronald J. Parrington, Joseph O. Maciejewski, James F. Lane, ASM International, 2024, p 140–153, https://doi.org/10.31399/asm.hb.v12.a0006946
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.