This article describes the general factors that can influence fracture appearances. The focus is on the general practical relationships of fracture appearances, with factors presented in some broad categories, including: material conditions (e.g., crystal structure and microstructure); loading conditions (stress state, strain rate, and fatigue); manufacturing conditions (casting, metal-working, machining, heat treatment, etc.); and service and environmental factors (hydrogen embrittlement, stress corrosion, temperature, and corrosion fatigue).