This article discusses several examples of fatigue load histories that intentionally create artificial fracture-surface markings during testing such that they are measurable by post-test quantitative fractography (QF). It reviews a number of methods for providing fatigue fracture-surface markers to aid QF of fatigue crack growth (FCG). These methods are based on load changes, including reordering the basic load histories and/or adding loads to them. The article also provides some guidelines for obtaining recognizable FCG markers for a variety of load histories and crack-growth regimes for coupons, components, and, particularly, full-scale fatigue tests.