This article discusses the importance of the care and handling of fracture specimens and what to look for during the preliminary field or laboratory observation and collection, the preservation of specimens, and the cleaning and preparation of fracture specimens for additional analyses. The preservation of nonmetallic specimens, medical devices, oversized components, light alloys, nondestructively tested components, and materials that are part of legal proceedings is addressed.