Introduction to Types and Appearances of Fracture
By
Ronald J. Parrington
Ronald J. Parrington
Applied Technical Services (ATS)
Search for other works by this author on:
-
Published:2024
Page range:
67 - 74
Abstract
This article addresses macroscale fracture appearances, microscale fracture-surface appearances or morphologies, fracture mechanisms, and those factors that influence fractures and fracture appearances. Some of the macroscopic and microscopic features identified by the failure analyst to evaluate the fracture surfaces of metals and plastics are described and compared.
You do not currently have access to this chapter.
Citation
Ronald J. Parrington, Introduction to Types and Appearances of Fracture, Fractography, Vol 12, ASM Handbook, Edited By Craig J. Schroeder, Ronald J. Parrington, Joseph O. Maciejewski, James F. Lane, ASM International, 2024, p 67–74, https://doi.org/10.31399/asm.hb.v12.a0006842
Download citation file:
Related Book Content
Martensitic Stainless Steels: Atlas of Fractographs
Fractography
Failure Analysis of a Wire Rope
ASM Failure Analysis Case Histories: Rail and Rolling Stock
Scanning Electron Microscopy in Fractography
Fractography
Fractography of Concrete
Fractography
Introduction to Quantitative Fractography
Fractography
Cast Aluminum Alloys: Atlas of Fractographs
Fractography
Copper Alloys: Atlas of Fractographs
Fractography
Examination of Fracture Surfaces
Fractography
Fractography of Weldments
Fractography