This article provides an overview of the supply chain for metallic additively manufactured materials, with an emphasis on spherical alloy powders. The article describes powder production processes as well as the various metal alloys that can be produced using powder AM techniques. It also reviews the basic characteristics of powder feedstocks and the management of metallic powders.
William Herbert, Ben Ferrar, Metal Additive Manufacturing Supply Chain, Powder Production, and Materials Life-Cycle Management, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 568–581, https://doi.org/10.31399/asm.hb.v24A.a0007021
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.