Standardization and the Use of Standards in Additive Manufacturing Available to Purchase
-
Published:2023
Abstract
This article presents the history of standardization in additive manufacturing (AM). It explains the need and structure for standardization in AM, including the application of AM standards by the industry sector. It also presents the primary purposes of these standards to create AM qualification and certification frameworks.
Shane Collins, Khalid Rafi, Standardization and the Use of Standards in Additive Manufacturing, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 541–547, https://doi.org/10.31399/asm.hb.v24A.a0006993