The aviation industry has been driving the use of additive manufacturing (AM), moving from one-off demonstrator or pathfinder components toward higher-volume serial production applications. This article presents an introduction to AM in aviation, explaining how aviation requirements apply to AM. It also presents advancements, standards, and future expectations of aviation.