Physics-Based Feedforward Control of Metal Additive Manufacturing
-
Published:2023
Abstract
Physics-based feedforward control is discussed in this article for two important laser-based metal additive manufacturing (AM) processes: directed-energy deposition and laser powder-bed fusion. For each type of process, control-oriented, lumped-parameter models that characterize melt pool dynamics as a function of process parameters are discussed first. Then, the derivation of model-based controllers is illustrated, followed by experimental evaluations of the model-based controller implemented as a feedforward control on a commercial AM system.
Qian Wang, Physics-Based Feedforward Control of Metal Additive Manufacturing, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 351–359, https://doi.org/10.31399/asm.hb.v24A.a0006986
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.