Review of Ultrasonic Testing for Metallic Additively Manufactured Parts Available to Purchase
-
Published:2023
Abstract
This article focuses on ultrasonic testing (UT) applied to metallic additive manufacturing (AM) parts, presenting the basic principles of UT. It provides a detailed discussion on postprocess UT inspection of powder-bed-fusion-manufactured samples and directed-energy-deposition-manufactured samples.
Ewen Carcreff, Nans Laroche, Anne-Françoise Obaton, Review of Ultrasonic Testing for Metallic Additively Manufactured Parts, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 310–323, https://doi.org/10.31399/asm.hb.v24A.a0006982