This article focuses on ultrasonic testing (UT) applied to metallic additive manufacturing (AM) parts, presenting the basic principles of UT. It provides a detailed discussion on postprocess UT inspection of powder-bed-fusion-manufactured samples and directed-energy-deposition-manufactured samples.