Nondestructive Testing in Additive Manufacturing—A Review
-
Published:2023
Abstract
This article covers defect formation and classification, followed by a brief description of the most common nondestructive testing (NDT) methods used for postbuild inspection. Descriptions of the established and emerging NDT techniques for in-process monitoring (IPM) and in-process inspection (IPI) in additive manufacturing (AM) also are provided, highlighting the advantages and limitations. The article concludes with a list of the main NDT methods and techniques used. As qualification and certification of AM parts is an urgent matter for the AM industry, a description of the current work carried out for developing standards is also included.
Wilson Vesga, Ben Dutton, Nondestructive Testing in Additive Manufacturing—A Review, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 287–302, https://doi.org/10.31399/asm.hb.v24A.a0007023
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.