FAIR Additive Manufacturing Data Management Principles Available to Purchase
-
Published:2023
Abstract
This article details findability, accessibility, interoperability, and reusability (FAIR) additive manufacturing data management principles and examines related motivations, benefits, and challenges. It explains opportunities to advance the state of the AM community efforts in fostering FAIR data management practices/principles and outlines the consequence of such efforts on technology maturation and industrialization for AM technologies.
William E. Frazier, Yan Lu, Paul Witherell, Alex Kitt, FAIR Additive Manufacturing Data Management Principles, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 171–176, https://doi.org/10.31399/asm.hb.v24A.a0006979
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.